Technical Parameters of Asphalt Thermal Recycling Mixing Plant | ||||||||
Type |
Production rate |
Measuring Accuracy |
Oil and Stone Ratio |
Fuel Consumption |
Temperature of Finished Materials |
Total Machine Power |
||
Aggregate Materials |
Powder Materials |
Asphalt |
||||||
LRB800 |
50~60t/h |
±1% |
±0.3% |
±0.2% |
2%~5% |
5~7kg/t |
140~160℃ |
340KW |
LRB1000 |
60~75t/h |
±1% |
±0.3% |
±0.2% |
2%~5% |
5~7kg/t |
140~160℃ |
441KW |
LRB1350 |
80~100t/h |
±1% |
±0.3% |
±0.2% |
2%~5% |
5~7kg/t |
140~160℃ |
441KW |
LRB1750 |
100~120t/h |
±1% |
±0.3% |
±0.2% |
2%~5% |
5~7kg/t |
140~160℃ |
536KW |